The ratio of single 6 to double 6 must be matched. The adjustment of the ratio of the seasons should be small, and the amount of the release agent should be adjusted according to the seasonal changes.
After the material is crushed, the proportion of addition should be controlled. It is not possible to mix too much in a single time. When black and color are added less and black, the choice of color master is very important.
The temperature of the injection molding can't make the staff adjust too high, so the cable ties that come out are all brittle, and the molecular structure of the nylon is completely destroyed, which has a great influence on the pulling force.
The mold clamping force, injection time, and glue injection time must be adjusted. The mold is now fully automatic, and the output is improved. However, attention should be paid to the air bubbles. The injection time is short, and the product is prone to bubbles and affects the appearance.
When changing the mold, the product should be tested one by one, especially for small specifications. Pay attention to whether there are any missing teeth, anti-tooth, eccentric and so on.